Home PageAbout MindatThe Mindat ManualHistory of MindatCopyright StatusWho We AreContact UsAdvertise on Mindat
Donate to MindatCorporate SponsorshipSponsor a PageSponsored PagesMindat AdvertisersAdvertise on Mindat
Learning CenterWhat is a mineral?The most common minerals on earthInformation for EducatorsMindat ArticlesThe ElementsThe Rock H. Currier Digital LibraryGeologic Time
Minerals by PropertiesMinerals by ChemistryAdvanced Locality SearchRandom MineralRandom LocalitySearch by minIDLocalities Near MeSearch ArticlesSearch GlossaryMore Search Options
The Mindat ManualAdd a New PhotoRate PhotosLocality Edit ReportCoordinate Completion ReportAdd Glossary Item
Mining CompaniesStatisticsUsersMineral MuseumsClubs & OrganizationsMineral Shows & EventsThe Mindat DirectoryDevice SettingsThe Mineral Quiz
Photo SearchPhoto GalleriesSearch by ColorNew Photos TodayNew Photos YesterdayMembers' Photo GalleriesPast Photo of the Day GalleryPhotography
╳Discussions
💬 Home🔎 Search📅 LatestGroups
EducationOpen discussion area.Fakes & FraudsOpen discussion area.Field CollectingOpen discussion area.FossilsOpen discussion area.Gems and GemologyOpen discussion area.GeneralOpen discussion area.How to ContributeOpen discussion area.Identity HelpOpen discussion area.Improving Mindat.orgOpen discussion area.LocalitiesOpen discussion area.Lost and Stolen SpecimensOpen discussion area.MarketplaceOpen discussion area.MeteoritesOpen discussion area.Mindat ProductsOpen discussion area.Mineral ExchangesOpen discussion area.Mineral PhotographyOpen discussion area.Mineral ShowsOpen discussion area.Mineralogical ClassificationOpen discussion area.Mineralogy CourseOpen discussion area.MineralsOpen discussion area.Minerals and MuseumsOpen discussion area.PhotosOpen discussion area.Techniques for CollectorsOpen discussion area.The Rock H. Currier Digital LibraryOpen discussion area.UV MineralsOpen discussion area.Recent Images in Discussions
Techniques for CollectorsSodium Dithionite Substitute for Waller's Solution
29th Jan 2005 18:45 UTCFranklin Roberts
Because Na Dithionite has two identical sulfur atoms, it can undergo two redox reactions. The second sulfur atom donates its available pair of electrons to another molecule of ferric oxy-hydroxide and the process repeats. The NaMBS oxidizes a second time to sodium dithionate (-ate, not -ite), and it is now completely oxidized.
The chemical formula for the two-stage reaction looks something like this:
1. Na-O-SO-SO-O-Na + Fe+++(O,OH) --> Na-O-SO2-SO-O-Na (NaMBS) + Fe++(OH)2
2. Na-SO2-SO-O-Na + Fe+++(O,OH) --> Na -O-SO2-SO2-O-Na + Fe++(OH)2
As you can see, making up Waller's solution with NaMBS instead of Na dithionite would work since it's an intermediate product of the reaction anyway. The only downside to using it is that you must use two molar equivalents of NaMBS versus one of the dithionite to achieve the same results. According to my Merck Index, Na dithionite has a molecular weight of 174.11 g/mole and NaMBS weighs in at 190.11 g/mole. (Notice that the metabisulfite salt weighs exactly 16 g/mole more than the dithionite, the weight of the added mole of oxygen from the first redox reaction.) In order to whip up a batch of Waller's solution with NaMBS, you will have to use 2.18 grams of NaMBS for every gram of Na dithionite called for in the recipe. It would probably be a good idea to add an extra 20% of distilled water to the formula to offset the increased tonicity of the solution resulting from the extra dissolved NaMBS.
Sodium metabisulfite should be a lot easier to buy than sodium dithionite, and it doesn't have that rotten egg smell either, although it does release sulfur dioxide if mixed with acids. (Just be sure to add the NaMBS to the citrate/bicarbonate buffer solution AFTER the bicarb has been added to prevent this.) Na MBS is used as a reducing agent for precipitating pure gold from aqua regia solutions and as a preservative in food and wine because its affinity for oxygen retards spoilage. In fact, those sulfite warning labels on wine bottles specifically refer to NaMBS. You should be able to buy it from any chemical supply or shop that caters to winemakers. You can also get it for USD $2.00/lb online at http://www.allseasonsnashville.com/beer%20and%20wine%20additives.htm It is sometimes referred to by its old name, sodium pyrosulfite. It can also be found on eBay. Just remember to seal the opened container or it will oxidize, just like Na dithionite will.
Franklin Roberts
Austin, Texas
6th Feb 2005 10:42 UTCLloyd L
I've been impressed with the effect that sodium dithionite solution has had on the few specimens on which I've so far tried it.
In the UK, sodium dithionite is quite difficult to procure, so if your recipe is as effective, or nearly as, then this is very useful information.
Thanks again,
Lloyd
14th Feb 2005 15:45 UTCMatthew Neuzil
14th Feb 2005 18:19 UTCJim
Sodium Metabisulfite 20-65%
Sodium Hydrosulfite 20-65%
(I wonder why the great variation in percentage?)
14th Feb 2005 20:32 UTCmatthew neuzil
15th Feb 2005 23:38 UTCFranklin Roberts
Franklin Roberts
Austin, Texas
15th Apr 2005 03:26 UTCandy christy
"In this case, the prefix "meta" which is Greek for "after" refers to the fact that the metabisulfite is the species that comes after sodium bisulfite (dithionite) in the chain of oxidation products going from sodium dithionite -> sodium metabisulfite -> sodium dithionate. "
Unfortunately, it does not. This usage of "meta" is similar to that in "metasilicate" for silicates with an 2- anion instead of "orthosilicate" for 2- stoichiometry. In that case, the hypothetical meta acid H2SiO3 is produced by removing H2O from the ortho acid H4SiO4. In the case of metabisulfite, one H2O is removed from two molecules of the hypthetical sulfurous acid H2SO3 to give equally hypothetical H2S2O5, of which NaMBS is the sodium salt.
Matthew Neuzil (Feb 14, 20:32):
"meta i would assume means it is hydrated like metatorbornite etc. "
No. The "meta" in "metatorbernite" implies LESS structural water than in "torbernite", same as above! But "meta" in many minerals is also used to indicate a polymorphic or alteration relationship that is not dehydration, eg metavariscite and variscite, which are polymorphs of the same composition.
Jim (Feb 14, 18:19):
"Matt, from an MSDS for Super Iron Out:
Sodium Metabisulfite 20-65%
Sodium Hydrosulfite 20-65%
(I wonder why the great variation in percentage?)"
Because Na hydrosulfite (= Na dithionite) absorbs oxygen readily from the air, to form metabisulfite, and the manufacturers refuse to guarantee precisely how much of it has turned already. They do suggest that the total of the two stays constant at around 85%. I suspect that the other 15% is dithionate, sulfate and adsorbed water. Even lab reagent dithionite is usually sold as about 85% or so rather than 99+%.
17th Nov 2010 09:34 UTCRock Currier Expert
I think it time that someone wrote up an article about the use of Waller solution/Sodium dithionite for cleaning "iron stains" off of minerals. I have used some of the information you have give us here on mindat in my article on cleaning quartz (credit given to you of course), but feel that is has now become such a commonly used method of cleaning iron minerals off of minerals that it really should have its own separate article. I could write it up, but I think you probably have more knowledge of its chemistry and perhaps more experience in than I in making it from scratch and its employment on various minerals than I. Would you consider writing such an article? As usual there is no reward other than your name on the article and the recognition that may come with that. I continue to be amazed as how much use some of these articles get. The one I wrote on cleaning quartz has so far generated something over 23K hits.
In your post you say: in the chain of oxidation products going from sodium dithionite ->. What does ->, mean? Google gives no meaningful hits.
12th Dec 2010 00:54 UTCFranklin Roberts
Sure, I'd be happy to write such an article. Why don't you PM me so we can coordinate our efforts. I'm still recuperating from my accident and won't be returning to work until after the holidays, so now would be a great time to tackle this project.
Frank
PS -> is what a right arrow becomes when posted to this forum. I've noticed that special characters and some punctuation gets mangled the same way. In order to read the chain of oxidation products correctly, just substitute a right arrow wherever you encounter ->
23rd Dec 2010 12:01 UTCJan Franek (2)
Honza Franek
30th Dec 2010 05:36 UTCPeter Haas
It's the concentration that makes the difference. The reaction of dithionite with atmospheric oxygen, or with any oxydant in general, is exothermic. In a dilute solution, and with water as the solvent which has a high specific heat capacity, the temperature increase is not substantial. With moisture in a pure dithionite powder, however, the solution will be saturated or at least close to the saturation point, so the heat production per unit volume will be orders of magnitude higher. Since the powder consists of solid particles with ambient air in interstitial spaces, and gases in general have a very low specific heat capacity, considerable temperatures are locally reached fairly easily. Temperature, however, increases the reaction rate, so the process is self-accelerating and the heat production increases exponentially. Above a certain temperature, dithionite starts to decompose even without an oxydant and the mixture explodes.
7th Jan 2011 12:37 UTCBarry Flannery Expert
For those who mightn't know about it: http://www.mindat.org/article.php/970/Guidelines+on+using+chemicals+to+clean+minerals
8th Jan 2011 03:30 UTCPeter Haas
A detailed guide on how to remove iron stains with dithionite is essentially contained in Rocks's article about cleaning quartz, which is available somewhere on this site.
8th Jan 2011 05:28 UTCE.Abbott
8th Jan 2011 07:17 UTCPeter Haas
Rock's article addresses the cleaning process in more detail and gives a wealth of practical tips that will help to "customize" it accprding to your personal needs.
8th Jan 2011 11:27 UTCRock Currier Expert
8th Jan 2011 14:02 UTCgord major
A member of the ROM staff told me Waller's soln was verboten caused by unavailability of sodium hydrosulphite, dithionite or sulfoxylate was difficult to obtain.
Since I have seen drums abet small outside the local dyehouse, so this suprised me
It is also used in water treatment Boilers I think and paper mills?
I would be suprised if it wasn't in toilet bowl cleaners esp. in high iron areas. I have used this.
I am more worried about the production of hydrogen sulphide
We used to be able to purchase "chemicals" from the druggist's ie chemist's to you Brit's
PC of big brother has eliminated this source and you have to have a account number from your local chemical supplier with everything but your maiden aunt's name.
Think of Ammonium nitrate except for Oppau it wasn't until 1947 it's explosive properties were recognized Thanks to Haber it is still produced safely in bulk esp. for gardeners
Thedifference between a medicine and a poison is the dose
Mindat.org is an outreach project of the Hudson Institute of Mineralogy, a 501(c)(3) not-for-profit organization.
Copyright © mindat.org and the Hudson Institute of Mineralogy 1993-2024, except where stated. Most political location boundaries are © OpenStreetMap contributors. Mindat.org relies on the contributions of thousands of members and supporters. Founded in 2000 by Jolyon Ralph.
Privacy Policy - Terms & Conditions - Contact Us / DMCA issues - Report a bug/vulnerability Current server date and time: April 26, 2024 17:56:48
Copyright © mindat.org and the Hudson Institute of Mineralogy 1993-2024, except where stated. Most political location boundaries are © OpenStreetMap contributors. Mindat.org relies on the contributions of thousands of members and supporters. Founded in 2000 by Jolyon Ralph.
Privacy Policy - Terms & Conditions - Contact Us / DMCA issues - Report a bug/vulnerability Current server date and time: April 26, 2024 17:56:48